Research Article
Plasma Treatment and TEOS Modification on Wood Flour Applied to Composite of Polyvinyl Chloride/Wood Flour
Table 2
TG characteristic of WF and WS samples.
| Characteristic | WF | WS1 | WS5 | WS10 |
| (°C) | 246 | 252 | 252 | 253 | (°C) | 414 | 421 | 423 | 429 | (°C) | 303 | 307 | 308 | 308 | The percent of weight retention (%) at 500°C | 0.2 | 0.4 | 2.6 | 3.7 |
|
|