Research Article
Epoxy-Glass Microballoon Syntactic Foams: Rheological Optimization of the Processing Window
Table 1
Characteristics of hollow glass microballoons [
2].
| HGM | Density (kgm−3) | Wall thickness (μm) | Radius ratio | Microballoon size (mean diameter) (μm) | Isostatic crush strength (MPa) | Thermal conductivity (Wm−1K−1) at 21°C |
| K15 | 150 | 0.70 | 0.9839 | 43.6 | 2 | 0.055 | K46 | 460 | 1.29 | 0.9356 | 40 | 41 | 0.153 |
|
|