Research Article
A Research on Modification Method for NSM FRP-Concrete Bonded Joints Strength Models
Table 3
Database under the adhesive-FRP interface failure mode.
| Reference | Number of tests | FRP material | fc (MPa) | Ef (GPa) | tp (mm) | tf (mm) | (mm) |
| [33] | 3 | CFRP | 36.199 | 37.17–174.17 | 11 | 11 | 14 | [24] | 2 | CFRP | 34.5 | 124 | 12 | 12 | 25 | [29] | 7 | GFRP/CFRP | 19 | 46–182 | 8 | 8 | 14–15 | [30] | 4 | GFRP/CFRP | 19 | 51–159 | 8–10 | 8–10 | 14–15 | [34] | 6 | BFRP/GFRP/CFRP | 36.2 | 40.8–155 | 6–10 | 6–10 | 5–15 | [35] | 6 | CFRP | 34.86 | 124–165 | 8–20 | 1.4–8 | 6–20 | [31] | 1 | CFRP | 19.6 | 155 | 8 | 8 | 14 | [36] | 2 | CFRP | 28.5 | 149–155 | 9.5 | 9.5 | 14.25–19 | Total | 31 | BFRP/GFRP/CFRP | 19–36.2 | 37.17–182 | 6–20 | 1.4–12 | 5–25 |
|
|