Microstructure, Tensile Property, and Surface Quality of Glass Fiber-Reinforced Polypropylene Parts Molded by Rapid Heat Cycle Molding
Table 2
Surface roughness of test samples.
| Roughness | Ra (μm) | Average | Sample | 1 | 2 | 3 | 4 | 5 |
| CIM | 0.944 | 1.042 | 0.668 | 0.636 | 0.895 | 0.837 | RHCM60 | 0.352 | 0.431 | 0.336 | 0.337 | 0.358 | 0.363 | RHCM90 | 0.181 | 0.234 | 0.212 | 0.189 | 0.216 | 0.206 | RHCM120 | 0.196 | 0.235 | 0.190 | 0.213 | 0.155 | 0.198 |
|
|