Specified parameters of continuous differential microemulsion polymerization.

CompositionsInitial microemulsion wt./wt., APS, water
Organic phaseMMA/dodecane =1 : 4

Operating conditionsFlow ratio,  mL/min
Temperature70–85°C
Prepolymerization time0–20 min