Research Article

Acrylonitrile-Styrene-Acrylate Particles with Different Microstructure for Improving the Toughness of Poly(styrene-co-acrylonitrile) Resin

Table 2

Glass transition temperature of ASA particles with different morphologies.

SampleCross-linkera (wt%)

ASA-C10.4-46.9111.7
ASA-C20.8-46.6111.9
ASA-C31.2-45.1112.4
ASA-C41.6-45.2112.2
ASA-C52.0-45.6111.5

aBased on the total amount of monomer in the fabrication process of PBA core. b, c, the glass transition temperature in low- and high-temperature regions is measured by DSC Q2000.