Research Article
Facile Production of Graphene/Polypropylene Composites with Enhanced Electrical and Thermal Properties through In Situ Artificial Latex Preparation
Table 3
Onset crystallization, crystallization peak and mass loss temperatures for neat PP and EOGr/PP composites.
| Sample | Crystallization peak temperature (°C) | Onset crystallization temperature (°C) | Weight loss temperature (°C) | 1% | 2% | 3% | Maximum |
| Neat PP | 96.8 | 106.3 | 335 | 359 | 365 | 443 | EOGr/PP-0.5 | 101.0 | 109.2 | 203 | 268 | 325 | 454 | EOGr/PP-1 | 102.5 | 110.6 | 216 | 256 | 288 | 455 | EOGr/PP-2 | 102.7 | 110.8 | 197 | 245 | 284 | 457 |
|
|