Research Article
Crystallization and Melting Behavior of UHMWPE Composites Filled by Different Carbon Materials
Table 4
The DSC data of oxidized UHMWPE composites.
| GO (wt%) | (°C) | (J·g-1) | (%) | (°C) | (J·g-1) | (°C) |
| 0 | 135.5 | 129.1 | 44.4 | 118.0 | 128.6 | 15.5 | 5 | 135.2 | 168.0 | 57.7 | 119.8 | 214.9 | 15.4 | 10 | 134.0 | 182.3 | 62.3 | 120.8 | 244.1 | 13.2 | 15 | 133.3 | 165.4 | 56.8 | 121.2 | 236.2 | 12.1 | 20 | 132.5 | 162.1 | 55.7 | 122.6 | 233.5 | 10.1 |
|
|