Specifications of the HP-DSC experiments.

PSP2VPP4VPPαMS

(°C)5050100140

(°C)200170220240

Test pressure (bar)10 - 30

1st segment (air atmosphere)(i) Heating: 25°C - with rate 10 K/min
(ii) Cooling: to

2nd segment (CO2 atmosphere)(i) Purging CO2, 20 mL/min for 5 min
(ii) , test pressure for 3 h
(iii) to with rate 10 K/min, test pressure