Research Article
Enrichment of Limestone Used in the Desulphurisation of Fluidised-Bed-Boiler Flue Gases
Table 3
Description of studied samples.
| Sample ID | Sample composition | Sample preparation |
| Sample 1 | 2 g of CaCO3 dr. 5 | Weighed and subsequently calcined | Sample 2 | 2 g of Sorbacal SP | Weighed and subsequently calcined | Sample 3 | 2 g of Sorbacal H 90 | Weighed and subsequently calcined | Sample 4 | 2.4 g of CaCO3 dr. 5 | Weighed and subsequently calcined (same as sample 1 but 20 wt. % more limestone) | Sample 5 | 2 g of Sorbacal SP | No calcination—weighed and inserted into the apparatus without calcination | Sample 6 | 2 g of Sorbacal H 90 | No calcination—weighed and inserted into the apparatus without calcination | Mixture A | 2 g of CaCO3 dr. 5 + 20 wt. % of Sorbacal SP | CaCO3 weighed and subsequently calcined, Sorbacal uncalcined | Mixture B | 2 g of CaCO3 dr. 5 + 20 wt. % Sorbacal H 90 | CaCO3 weighed and subsequently calcined, Sorbacal uncalcined |
|
|