Research Article
Photocatalytic Degradation of Methyl Green Dye Mediated by Pure and Mn-Doped Zinc Oxide Nanoparticles under Solar Light Irradiation
Table 1
The estimation of crystallite size and microstrain in pure and Mn-doped ZnO samples using the W-H method.
| Parameters | Peak position | FWHM | -axis | -axis | -intercept | Crystallite size | Microstrain (Є) | | λ(Å) | 2θ (deg) | (deg) | | | (nm) | No unit |
| Structural parameters for pure ZnO XRD’s data using Williamson-Hall plot | 0.94 | 1.5406 | 36.20237 | 0.49032 | 1.242784353 | 0.008134172 | 0.00657 | 21.10410959 | | | | 34.3841 | 0.42664 | 1.182301995 | 0.007113569 | | | | | | 31.7238 | 0.46896 | 1.093278514 | 0.007873242 | | | | | | 47.47716 | 0.51164 | 1.61025698 | 0.008174267 | | | | | | 56.53489 | 0.51897 | 1.89435141 | 0.007977569 | | | | | | 62.78453 | 0.57248 | 2.083577587 | 0.008529093 | | | | | | 67.87294 | 0.62157 | 2.233093267 | 0.009000488 | | | | | | 68.99383 | 0.60138 | 2.265447449 | 0.008650399 | | | |
| Structural parameters for Mn-doped ZnO XRD’s data using Williamson-Hall plot | 0.94 | 1.5406 | 36.36538 | 0.59023 | 1.2481916 | 0.009787068 | 0.00739 | 18.7623816 | | | | 34.54185 | 0.47705 | 1.1875614 | 0.007950683 | | | | | | 31.90264 | 0.56533 | 1.0992822 | 0.009486951 | | | | | | 47.60118 | 0.65403 | 1.6142189 | 0.010444196 | | | | | | 56.66233 | 0.67434 | 1.8982682 | 0.010359701 | | | | | | 62.88501 | 0.74308 | 2.0865708 | 0.011064849 | | | | | | 67.96516 | 0.7939 | 2.2357633 | 0.01148964 | | | | | | 69.10656 | 0.67618 | 2.2686894 | 0.009719761 | | | |
|
|