Research Article

The Bioactivated Interfacial Behavior of the Fluoridated Hydroxyapatite-Coated Mg-Zn Alloy in Cell Culture Environments

Figure 2

Typical XRD diffraction pattern. (a) The result on the Mg-Zn alloy after 14 days’ culture and detaching the cells from the sample. (b) The result on the FHA-coated one. Curve-a presents the diffraction pattern of the FHA coatings right after the electrodeposition. Curve-b presents the pattern of the FHA coatings after being immersed in m-SBF for 14 days. Curve-c presents the diffraction pattern of the FHA coatings after 14 days’ culture in cell culture environment and detaching the cells from the sample.
192671.fig.002a
(a)
192671.fig.002b
(b)