Corrosion Performance of Fe-Cr-Ni Alloys in Artificial Saliva and Mouthwash Solution
Table 4
Electrochemical parameters of the materials evaluated in mouthwash at 37°C.
| Material | (mV) | (mV/Dec) | (mV/Dec) | (mA/cm2) |
| 304-H | 317 | 581 | 133 | 0.001713 | 309-H | 330 | 356 | 129 | 0.00111 | 310-H | 333 | 306 | 121 | 0.00127 | 316-H | 302 | 642 | 140 | 0.0023 | 321-H | 304 | 333 | 138 | 0.0027 | 347-H | 310 | 371 | 126 | 0.0021 | Titanium | −96 | 356 | 176 | 0.0116 |
|
|