(a)
(b)
Figure 1: UV-Vis spectra recorded at different time intervals for nanoparticle formation using GSTE at 100°C with (a) 1 mM H2PtCl6·6H2O solution and (b) 1 mM PdCl2 solution. Control represents corresponding salt solution without GSTE.