Biomechanical properties of the fresh amnion and the AHAM.

ParameterFresh HAMAHAM 𝑡 value 𝑃 value

Sample ( 𝑛 )1212
Thickness (mm) 0 . 1 6 4 ± 0 . 0 0 6 0 . 1 4 3 ± 0 . 0 0 5 𝑡 = 9 . 4 2 𝑃 = 0 . 0 0
Transitional stress (MPa) 0 . 1 4 4 ± 0 . 0 3 7 0 . 1 4 2 ± 0 . 0 2 6 𝑡 = 1 . 8 3 𝑃 = 0 . 0 8
Transitional strain (%) 1 1 . 8 0 8 ± 0 . 8 3 3 1 2 . 2 0 0 ± 0 . 9 5 9 𝑡 = 1 . 0 7 𝑃 = 0 . 3 0
Failure strain (MPa) 0 . 8 2 0 ± 0 . 0 2 8 0 . 7 9 6 ± 0 . 0 4 5 𝑡 = 1 . 5 7 𝑃 = 0 . 1 3
Failure strain (%) 3 2 . 6 9 5 ± 1 . 5 6 0 3 3 . 7 7 7 ± 1 . 3 5 9 𝑡 = 1 . 8 1 𝑃 = 0 . 0 8