Biaxial Flexural Strength of High-Viscosity Glass-Ionomer Cements Heat-Cured with an LED Lamp during Setting

1Department of Dental Materials, Dental Faculty, National University of Córdoba, Maya de la Torre s/n, 5000 Córdoba, Argentina
2Department of Global Oral Health, College of Dental Sciences, Radboud University Nijmegen Medical Centre, P.O. Box 9101, 6500 HB Nijmegen, The Netherlands

Received 25 April 2013; Accepted 26 May 2013

Academic Editor: Xiupeng Wang

Copyright © 2013 Gustavo Fabián Molina et al. This is an open access article distributed under the Creative Commons Attribution License, which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.

How to Cite this Article

Gustavo Fabián Molina, Ricardo Juan Cabral, Ignacio Mazzola, Laura Brain Lascano, and Jo E. Frencken, “Biaxial Flexural Strength of High-Viscosity Glass-Ionomer Cements Heat-Cured with an LED Lamp during Setting,” BioMed Research International, vol. 2013, Article ID 838460, 6 pages, 2013. doi:10.1155/2013/838460