Review Article

Carbon Nanotubes Reinforced Composites for Biomedical Applications

Figure 7

Enlarged image of the border between the specimen and the bone (200x). (a and e) Alumina ceramic was implanted after 12 weeks (40x, 220x); (b and f) CNTs/alumina composite was implanted after 12 weeks (40x, 220x); (c and g) alumina ceramic was implanted after 24 weeks (40x, 220x); (d and h) CNTs/alumina composite was implanted after 24 weeks (40x, 220x) [97].
518609.fig.007a
(a)
518609.fig.007b
(b)
518609.fig.007c
(c)
518609.fig.007d
(d)
518609.fig.007e
(e)
518609.fig.007f
(f)
518609.fig.007g
(g)
518609.fig.007h
(h)