Research Article
An Alumina Toughened Zirconia Composite for Dental Implant Application: In Vivo Animal Results
Table 2
Dynamic mechanical tests.
| | A-04 | A-05 | A-06 |
| Flexural moment (Nmm) | | | | mean | 586.7 | 566.2 | 567.1 | dyn | 480.0 | 463.3 | 464.0 | max | 1066.8 | 1029.5 | 1031.0 | min | 106.7 | 102.9 | 103.1 | Compression force (N) | | | | mean | 95.4 | 95.7 | 95.5 | dyn | 78.0 | 78.3 | 79.0 | max | 173.4 | 174.1 | 175.5 | min | 17.3 | 17.4 | 17.5 |
|
|