Research Article
In Vivo Osseointegration Performance of Titanium Dioxide Coating Modified Polyetheretherketone Using Arc Ion Plating for Spinal Implant Application
Figure 5
Shear strength between bone tissues and implant for the three implants at 4, 8, and 12 weeks after implantation. compared to PEEK implant at 4 weeks after implantation.