Fracture Strength of Aged Monolithic and Bilayer Zirconia-Based Crowns
Figure 4
SEM micrograph of porcelain fractured surface showing critical flaw (crack) in bilayer (BL) veneered fractured crown. Note chipping at the occlusal surface (a) and voids inside veneering layer (b).