Research Article
LED Curing Lights and Temperature Changes in Different Tooth Sites
Figure 5
Characteristic (°C) versus time curves caused by irradiation with VALO (Ultradent), tested at a light intensity of 1000 (for 20 s) (a) or 3200 (for 3 s) mW/cm2 (b) during composite polymerization. B (bottom of the box); C (occlusal surface); D (mesial); E (pulp chamber).
(a) |