Evaluation of Mechanical Properties and Marginal Fit of Crowns Fabricated Using Commercially Pure Titanium and FUS-Invest
Table 1
Elasticity modulus, yield strength, tensile strength, and elongation of the specimens.
| | Elasticity modulus , GPa | Yield strength , MPa | Tensile strength , MPa | Elongation , % |
| 1 | 116.8 | 555.7 | 643.3 | 4.4 | 2 | 142.5 | 573.8 | 687.8 | 4.5 | 4 | 122.3 | 582.3 | 679.8 | 4.9 |
| 5 | 124.6 | 560.5 | 672.3 | 4.7 | 6 | 123.4 | 557.4 | 678.4 | 4.6 | 7 | 123.8 | 575.3 | 665.3 | 4.5 |
| Mean ± SD | 125.6 (8.8) | 567.5 (11.1) | 671.2 (15.6) | 4.6 (0.2) |
|
|