Research Article
Preparation of P3HB4HB/(Gelatin + PVA) Composite Scaffolds by Coaxial Electrospinning and Its Biocompatibility Evaluation
Figure 2
Surface roughness of the P3HB4HB/(GEL + PVA) scaffolds. (a) Roughness profile (); (b) roughness height (); (c) distance between contour peak line and contour bottom line (). A: GEL : PVA = 0.6 g : 0.2 g; B: GEL : PVA = 0.4 g : 0.4 g; C: GEL : PVA = 0.2 g : 0.6 g. .
(a) |
(b) |
(c) |