Research Article

Preparation of P3HB4HB/(Gelatin + PVA) Composite Scaffolds by Coaxial Electrospinning and Its Biocompatibility Evaluation

Figure 8

CCK-8 assay shows the proliferation of hBMSCs on days 1, 3, 5, 7, and 9  for the scaffold materials Group A: GEL : PVA = 0.6 g : 0.2 g; Group B: GEL : PVA = 0.4 g : 0.4 g; Group C: GEL : PVA = 0.2 g : 0.6 g. Compare to Group A: ; ; compare to Group B: ; .