BioMed Research International / 2018 / Article / Tab 1 / Research Article
Assessment the Bond Strength of Ceramic Brackets to CAD/CAM Nanoceramic Composite and Interpenetrating Network Composite after Different Surface Treatments Table 1 Materials used in the present study.
Materials Brand Names Manufacturer Lot Interpenetrating network composite (IPN) Vita Enamic (VE) Vita Zahnfabrik, Cuxhaven, Germany 41470 Nano-ceramic composite (NCC) Lava Ultimate (LU) 3M ESPE Dental Products, St. Paul, MN, USA N613657 Mandibular incisor ceramic brackets Damon Clear Ormco Corp, Orange, CA, USA 051766799 Acrylic resin Paladent Heraeus Kulzer GmbH, Grüner Weg, Hanau, Germany 012427 Hydrofluoric acid Ultradent Porcelain Etch Ultradent Products, South Jordan, UT, USA BCB97 Silane Ultradent Silane Ultradent Products, South Jordan, UT, USA BDVRD Orthodontic adhesive Transbond XT 3M Unitek, Monrovia, CA, USA HV4ZV