Research Article

Assessment the Bond Strength of Ceramic Brackets to CAD/CAM Nanoceramic Composite and Interpenetrating Network Composite after Different Surface Treatments

Table 3

Frequency distribution of Adhesive Remnant Index (ARI) scores and Chi-square test results.

MaterialSurfaceARI ScoresAsymp.
Treatments0123Sig. (2-sided)

Lava Ultimate (LU)1 W Laser21000
2 W Laser01200
Sandblast066026.0430.001
Silane3900
HF0930

Vita Enamic (VE)1 W Laser11100
2 W Laser01200
Sandblast075030.1100.000
Silane6600
HF3720