Effect of MDP-Based Primers on the Luting Agent Bond to Y-TZP Ceramic and to Dentin
Figure 2
Representative micrographs of the debonded surfaces: (a) mixed failure – residue of cement left on the left side of the debonded surface from Z-Prime Plus only group; (b) mixed failure exhibiting dentin tubules and cement from SB + Z-Prime Plus group.