Research Article

Effect of Surface Coating on Bond Strength between Etched Feldspar Ceramic and Resin-Based Luting Agents

Table 2

Estimates (95% confidence intervals) for mean microshear bond strength (μSBS), characteristic strength (σ0), and Weibull modulus (m).

GroupμSBS (MPa)σ0 (MPa)m

S-RC24.2 (21.8–26.726.5 (23.8–29.44.4 (3.2–6.0
SB-RC26.3 (24.2–28.528.3 (26.0–30.85.6 (4.1–7.7
UA-RC14.4 (12.3–16.616.1 (13.8–18.73.1 (2.3–4.3
S-F30.5 (28.5–32.532.4 (30.6–34.28.4 (5.9–12.0
SB-F22.8 (20.4–25.324.7 (22.7–27.05.3 (3.7–7.7
UA-F18.2 (16.4–20.019.8 (17.9–21.84.7 (3.4–6.6

Distinct letters in the same column indicate significant differences between groups.