Table 3: Strain amplification factor comparisons between this study and previous studies.

SourcesMethodStrain amplification factor

Present methodFEM (poroelastic)4.3
[24]FEM (linearly isotropic)3.14
[62, 63]In vitro measurement3.99–11.43