Improvement of the Shock Absorption Ability of a Face Guard by Incorporating a Glass-Fiber-Reinforced Thermoplastic and Buffering Space

Table 1

Materials used in the present study.

TypeSample labelProduct nameManufacturerCompositionBuffering spaceThickness (mm)Weight

Commercial medical splintAP32Rolyan Aquaplast-THomecraft RolyanPolycaprolactone×3.254.5 ± 0.6
AP16×1.638.3 ± 0.4
Experimental materialsAP-APSAP16 (50 × 50 mm)+ APS (100 × 100 mm)Min 1.6–Max 3.241.2 ± 0.1
GF-APSGF (50 × 50 mm) + APS (100 × 100 mm)Min 1.6–Max 3.241.6 ± 0.2

APS: AP16 with buffering space (APS); GF: glass-fiber-reinforced plastics (AP + glass fiber cloth (4 sheets)). Sample size: 100 × 100 mm, including cushioning materials.