Research Article

Properties Investigation of GO/HA/Pt Composite Thin Film

Table 1

Current density, , and corrosion potential, , obtained from PDS measurements for an uncoated substrate and HA, HA/GO, and HA/GO/Pt coatings on zirconium after 7 days.

Time/dayUncoated substrateHA coatingHA/GO coatingHA/GO/Pt coating

/nA
7279.60272.150.04427.227
/mV
7-21.699164.574267.02499.325