Research Article

Effects of 16% Carbamide Peroxide Bleaching on the Surface Properties of Glazed Glassy Matrix Ceramics

Table 3

Mean (SD) values of microhardness testing.

ā€‰e.max CADEmpress CADTotal

Control539,7 (16,4)525,6 (21,3)532,7 (19,7)
%16 CP530,3 (17,3)514,6 (22,2)522,5 (20,8)
Total535,0 (16,9)520,1 (21,7)527,6 (20,5)