Research Article

Effects of 16% Carbamide Peroxide Bleaching on the Surface Properties of Glazed Glassy Matrix Ceramics

Table 4

Two-way analysis of variance for surface roughness testing.

SourceType III sum of squaresdfMean squareF

Ceramic0,24110,2415,6990,025
Surface treatment2,04112,04148,179<0,001
Ceramic  surface treatment0,01010,0100,2460,625

represents significant difference.