Research Article

A New Type of Biphasic Calcium Phosphate Cement as a Gentamicin Carrier for Osteomyelitis

Figure 3

FTIR spectra of α-TCP/HAP biphasic cement containing (a) 0 wt%; (b) 4 wt%; (c) 16 wt% gentamicin sulfate immersed in distilled water for 15 minutes, 72 hours, 120, and 168 hours.
801374.fig.003a
(a)
801374.fig.003b
(b)
801374.fig.003c
(c)