Research Article

Laboratory Leaching Tests to Investigate Mobilisation and Recovery of Metals from Geothermal Reservoirs

Figure 13

Elemental composition (in ppm) of each leachate from samples reacted with deionised water at 200°C temperature under 250 bar pressure in the flow-through reactor after 52 minutes, 48 minutes, and 25 minutes, respectively (absence of data points reflects concentrations below the limits of detection).