Static uniaxial compression test results for specimens with different chemical solutions.

Specimen groupNumberStatic UCS/MPaStatic elastic modulus (GPa)
TestedAverageTestedAverage

H2SO4A752.6751.378.768.76
A851.158.70
A950.288.82

Distilled waterB761.1461.049.739.68
B861.629.70
B960.379.60

NaOHC751.1352.539.129.06
C852.829.00
C953.659.05

NaturalD763.8663.3610.4510.34
D863.4310.30
D962.7910.28