Research Article
Performance of Ecological Pervious Concrete Prepared with Sandstone/Limestone-Mixed Aggregates
Table 7
Water retention of the ecological pervious concrete.
| Test blocks | After drying/kg | After immersion in water/kg | Soak dry/kg | Water absorption per unit mass |
| 0% sandstone aggregate | 1.6517 | 1.6710 | 0.0193 | 0.0117 | 25% sandstone aggregate | 1.6035 | 1.6316 | 0.0281 | 0.0175 | 50% sandstone aggregate | 1.3641 | 1.4243 | 0.0602 | 0.0441 | 75% sandstone aggregate | 1.3362 | 1.3962 | 0.0600 | 0.0449 | 100% sandstone aggregate | 1.3085 | 1.3676 | 0.0591 | 0.0452 |
|
|