Determination of Au in CMC ore sample and Gold Ore (MA-1b) CRM.
| Samples | Au concentration | Corrected values according to 97% desorption | (mgkg−1) |
| CMC sample | | | Au (found) | < LOD | < LOD | Au (claimed) | 1.34 | 1.34 | Au (spiked found) | 13.6 ± 0.6 | 14.1 ± 0.6 | Au (spiked) | 15 | 15 | Gold Ore (MA-1b) | | | Au (found) | 15.0 ± 1.0 | 15.5 ± 1.0 | Au (certified value) | 17.0 ± 0.3 | 17.0 ± 0.3 |
|
|
Values are given as mean ± SD, N = 3 (number of replicates). |