Performance Evaluation of STARPAM Polymer and Application in High Temperature and Salinity Reservoir
Table 7
The relationship between viscosity retention rate and aging time of three polymers.
| Place time /(d) | Viscosity retention rate /(%) | STARPAM | MO-4000 | HPAM |
| 0 | 100.00 | 100.00 | 100.00 | 1 | 111.47 | 102.62 | 104.96 | 3 | 108.18 | 99.92 | 96.49 | 7 | 106.50 | 94.56 | 92.93 | 15 | 99.88 | 91.69 | 90.20 | 30 | 95.65 | 88.68 | 87.47 | 60 | 90.49 | 82.63 | 81.09 |
|
|