Research Article
Effect of Reinforcement Fiber Arrangement on Thermal and Mechanical Properties of High Silica/Phenolic Resin Insulation Layer
Table 2
EDS results of the surface bonded to the throat.
| Species | Before the test (%) | After the test (%) | Change value (%) |
| C | 53.41 | 30.93 | -22.48 | O | 34.01 | 39.03 | +5.02 | Si | 11.08 | 27.51 | +16.43 | Al | 0.57 | 1.09 | +0.52 | Mg | 0.31 | 0.61 | +0.3 | Na | 0.63 | 0.82 | +0.19 |
|
|