Research Article
Effect of Reinforcement Fiber Arrangement on Thermal and Mechanical Properties of High Silica/Phenolic Resin Insulation Layer
Table 3
EDS results of the crack.
| Species | Before the test (%) | After the test (%) | Change value (%) |
| C | 53.16 | 31.99 | -21.17 | O | 20.84 | 44.92 | +24.08 | Si | 24.36 | 22.46 | -1.9 | Al | 0.48 | 0.37 | -0.11 | Mg | 0.39 | 0.27 | -0.12 | Na | 0.76 | 0 | -0.76 |
|
|