Research Article

Efficient Design of Flexible and Low Cost Paper-Based Inkjet-Printed Antenna

Table 2

Effect of 2-layer and 3-layer printing under exposure to temperature on resistance in Ω/cm.

Time (min)Resistance (Ω)

2-layer, temp. = 25°C
020 M
57
105.4
155.3
204.6
254.1

2-layer, temp. = 75°C
020 M
5500 K
10160 K
15164
20150
25130

3-layer, temp. = 25°C
020 M
59
108.8
157.2
205.8
255.6

3-layer, temp. = 75°C
020 M
5860 K
10420 K
15200
20192
25170