Research Article
Studies on Poly(propylene fumarate-co-caprolactone diol) Thermoset Composites towards the Development of Biodegradable Bone Fixation Devices
Table 8
Mechanical properties of cross-linked materials aged in PBS medium.
| Cross-linked materials | Load at maximum (kN) | Compressive strength (MPa) | Percent age loss of compressive strength | Compression modulus (MPa) | Percentage loss of compressive modulus |
| PPF-PL/nvp | 0.474 0 .07 | 16.754 2.32 | 90.55 | 182.129 74.16 | 84.27 | PPF-PL/nvp/K F | 0.384 0 .07 | 13.587 2.39 | 92.19 | 78.723 10.13 | 90.09 | PPF-PL/nvp/HA | 1.849 0 .42 | 65.388 15.03 | 62.23 | 421.877 51.07 | 77.21 |
|
|