Temperature-Responsive Gelation of Type I Collagen Solutions Involving Fibril Formation and Genipin Crosslinking as a Potential Injectable Hydrogel
Figure 12
Storage modulus () of the 0.25% PSC/10 mM genipin solution measured by a temperature-responsive gelation test. The numbers in the figure indicate the elapsed days after the preparation of genipin solution. The curves obtained at 37°C after the intervals of 600 s at 25°C were depicted.