Research Article

Fabrication of TiO2 Crystalline Coatings by Combining Ti-6Al-4V Anodic Oxidation and Heat Treatments

Figure 1

Macrographs and micrographs of anodically oxidized samples at 20, 40, and 60 V, with and without subsequent heat treatment at 500 and 600°C.
(a) TiG5
(b) 500
(c) 600
(d) 20
(e) 20-500
(f) 20-600
(g) 40
(h) 40-500
(i) 40-600
(j) 60
(k) 60-500
(l) 60-600