Research Article
Fabrication of TiO2 Crystalline Coatings by Combining Ti-6Al-4V Anodic Oxidation and Heat Treatments
Table 2
Roughness values,
, of the samples.
| Sample | [μm] |
| TiG5 | 0.020 | 20 | 0.019 | 40 | 0.020 | 60 | 0.018 | 500 | 0.021 | 20-500 | 0.017 | 40-500 | 0.025 | 60-500 | 0.030 | 600 | 0.029 | 20-600 | 0.030 | 40-600 | 0.030 | 60-600 | 0.040 |
|
|