Research Article

Fracture Resistance of Endodontically Treated Maxillary Premolars Restored by Various Direct Filling Materials: An In Vitro Study

Table 1

The comparison of the average values for resistance between the groups.

ABCDEFGH

Mean1289.00181.75445.38645.88355.13352.00191.38572.00
SD257.7557.9823.7538.4337.2326.3460.9861.82
Min972113405584300326124475
Max1700267468688404404277617

variance ratio) = 100,034798,  P < 0,0001
A (intact), B (unfilled), C (composite oblique layering), D (composite cusp coverage), E (bulk fill), F (glass-ionomer), G (amalgam), H (proximal box cavity).