Research Article
Preparation and Evaluation of Gelatin-Chitosan-Nanobioglass 3D Porous Scaffold for Bone Tissue Engineering
Table 1
Component of prepared scaffolds.
| Specimen name | Gel concentration (w/w) % | Chitosan concentration (w/w %) | CS-Gel/BG ratio (w/w) % | Solid loading (%) |
| GCB-0 | 30 | 70 | 100/0 | 40 | GCB-10 | 30 | 60 | 90/10 | 40 | GCB-20 | 30 | 50 | 80/20 | 40 | GCB-30 | 30 | 40 | 70/30 | 40 |
|
|