Research Article

Preparation and Evaluation of Gelatin-Chitosan-Nanobioglass 3D Porous Scaffold for Bone Tissue Engineering

Table 4

Pore diameter and porosity of composite scaffold.

Sample nameAverage pore diameter (μm)Porosity

BCG 0400 ± 13.689.3 ± 7.8
BCG 10250 ± 26.382.4 ± 5.0
BCG 20160 ± 17.880.8 ± 3.3
BCG 30100 ± 25.981.3 ± 6.1