Research Article
Enhancement of the Mechanical Properties of Hydroxyapatite/Sulphonated Poly Ether Ether Ketone Treated Layer for Orthopaedic and Dental Implant Application
Figure 6
The effect of compression on the horizontal load/scratch distance with (a) 3-, (b) 5-, and (c) 10-minute sulphonation time.
(a) |
(b) |
(c) |